Sign In | Join Free | My insurersguide.com
China Yuhong Group Co.,Ltd logo
Yuhong Group Co.,Ltd
Yuhong Holding Group Co.,LTD
Verified Supplier

13 Years

Home > Others >

ASTM A240 Stainless Steel 904L Plate With High Resistance To Stress Corrosion Cracking

Yuhong Group Co.,Ltd
Trust Seal
Verified Supplier
Credit Check
Supplier Assessment
Contact Now

ASTM A240 Stainless Steel 904L Plate With High Resistance To Stress Corrosion Cracking

Brand Name : YUHONG

Model Number : ASTM A240 904L

Certification : ABS, GL, DNV, NK, PED, AD2000, GOST9941-81, CCS, ISO 9001-2008

Place of Origin : CHINA

MOQ : 1pcs

Price : Negotiable

Payment Terms : L/C, T/T

Supply Ability : 1000Tons/Month

Delivery Time : 7DAYS

Packaging Details : Ply-wooden Case /Iron Case/ Bundle with plastic Cap

Product Name : Stainless Steel Plate, Sheet

Standard : ANSI, ASTM, ASME, JIS, DIN, EN

Material : Stainless Steel 904L

Width : As Resquest

Finish : Polished, Mirror, Bright, Hairline, Satin, Brushed, Ect.

Packing : Water Proof And Seaworthy Package

Contact Now

ASTM A240 904L NO8904 Stainless Steel Plate Sheet Coil

ASTM A240 is a specification for stainless steel plate, sheet, and strip for pressure vessels and for general applications. It covers grades such as 304, 304L, 316, 316L, 321, 347, and 904L.

Stainless steel 904L is a low carbon, high alloy austenitic stainless steel with excellent corrosion resistance. It is commonly used in chemical processing, oil and gas production, and other demanding environments where corrosion resistance is critical.

ASTM A240 stainless steel 904L plate is available in various thicknesses, widths, and lengths. It is typically supplied in the annealed condition and can be further heat treated to enhance its properties.

The mechanical properties of ASTM A240 stainless steel 904L plate include a tensile strength of 490 MPa (71 ksi), a yield strength of 220 MPa (32 ksi), and an elongation of 35%.

The execution standard for 904L seamless steel pipe is ASTM A240/ASME
904L belongs to austenitic stainless steel, with physical and mechanical properties: density: 8.24g/cm3. Tensile strength: σ B ≥ 520Mpa. Elongation: δ≥ 35%.It has good resistance to spot corrosion and Crevice corrosion, high resistance to stress corrosion cracking, good resistance to intergranular corrosion, good workability and weldability.

904L is a low-carbon austenitic stainless steel that can be used under severe corrosion conditions. It contains 25% nickel and 4.5% molybdenum, and has good resistance to chloride stress corrosion cracking. Compared with 316L and 317L, 904L has excellent corrosion resistance. Due to the addition of Cu, the alloy exhibits excellent corrosion resistance to reducing acids such as sulfuric acid and phosphoric acid.
Common applications include the production and transportation of sulfuric acid, metal pickling in sulfuric acid, papermaking and related industries, and the chemical and pharmaceutical industries.

ASTM A240 SS904L Stainless Steel Plate Chemical Composition

Element SS 904L
C 0.020 max
Mn 2 max
Si 1 max
P 0.040 max
S 0.030 max
Cr 19 – 23
Ni 23 – 28
Mo 4 – 5
Cu 1 – 2

ASTM A240 SS904L Stainless Steel Plate Mechanical Properties

Element SS 904L
Density 7.95 g/cm3
Melting Point 1350 °C (2460 °F)
Tensile Strength Psi – 71000 , MPa – 490
Yield Strength (0.2%Offset) Psi – 32000 , MPa – 220
Elongation 35%

Material Testing

1. Chemical processing

2. Oil and gas industry

3. Desalination plants

4. Food processing industry

5. Marine industry

6. Heat exchangers

7. Petrochemical industry

ASTM A240 Stainless Steel 904L Plate With High Resistance To Stress Corrosion Cracking


Product Tags:

ASTM A240 Stainless Steel Plate

      

High Resistance Stainless Steel Plate

      

Stress Corrosion Cracking Stainless Steel Plate

      
Cheap ASTM A240 Stainless Steel 904L Plate With High Resistance To Stress Corrosion Cracking for sale

ASTM A240 Stainless Steel 904L Plate With High Resistance To Stress Corrosion Cracking Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: Yuhong Group Co.,Ltd
*Subject:
*Message:
Characters Remaining: (0/3000)